1. Clean the aluminum partitions for use.

2. Put the butyl hot melt sealant into the extruder cylinder and preheat it to 130-140°C. After the thermostat is kept at a constant temperature, apply a strip of rubber to check the uniform line and apply the strip to the aluminum spacer groove. , After a little cool and clean glass pressure synthetic hollow glass semi-finished products.

3. After the outer sealant has been applied and cured, it will be the finished hollow glass product.

4. When using the imported fast-squeeze glue machine, the temperature of the rubber tube should be increased by 10-15°C, and the extrusion pressure should be adjusted from 150Mpa to 170-200Mpa.

Caution: When using butyl hot melt sealant, keep hands clean. Do not apply dust, oil and solvents (such as acetone, gasoline, etc.) to the surface of the adhesive. When touching hot glue, be careful of scalding. The gloves that touch the glue should be clean and free from burrs or other contaminants that are easily stuck on the glue. When butyl hot melt sealant is used, it should be controlled below 160°C. It is strictly forbidden to apply glue above 170°C in order to avoid degradation of the glue.

Purchase material glass

Amalgam UV Lamp

Replacement Uv Lamp,,Uvc Disinfection Lamp ,Amalgam Uv Light ,Germicidal Uvc Lamp

Foshan Kingrate Optoelectronic Technology Co., Ltd. , https://www.kingrateuv.com